321 stainless steel pipe and tube (UNS S32100)
321 (UNS S32100, EN 1.4541) is a titanium-stabilised austenitic grade that resists intergranular corrosion after welding and performs in continuous service up to about 870 °C. Used for exhaust systems, heat exchangers and refinery piping.
- Grade
- 321
- Stabiliser
- Titanium ≥ 5×C
- Standard
- ASTM A312, A240
- Lead time
- 7–15 days
321 specification summary
| Grade | 321 (UNS S32100) |
|---|---|
| European designation | EN 1.4541 |
| Japanese designation | SUS321 |
| Product standard | ASTM A312/A312M (pipe), ASTM A240/A240M (plate) |
| Form supplied | Seamless pipe, welded pipe, tube |
| Typical size range | Quoted per order — outside diameter, wall thickness and length confirmed on the quotation |
| Surface | Pickled, bright annealed, polished |
| Ends | Plain, bevelled, threaded on request |
| Certification | EN 10204 3.1 mill test certificate with each shipment |
| Packaging | Hexagonal bundle, wooden case or as specified |
Typical ranges are shown for guidance. Confirm the exact thickness, width, length and tolerance on the quotation before ordering; the mill certificate that arrives with the goods states the values actually supplied.
Chemical composition
| Grade | C max | Mn max | P max | S max | Si max | Cr | Ni | Ti | N max |
|---|---|---|---|---|---|---|---|---|---|
| 321 | 0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 17.0–19.0 | 9.0–12.0 | 5×(C+N) min, 0.70 max | 0.10 |
Values are standard limits for the designation, not a statement about a specific heat. The mill certificate states the measured composition of the material supplied.
Mechanical properties
| Grade | Tensile strength, min | Yield strength 0.2%, min | Elongation in 50 mm, min | Hardness, max |
|---|---|---|---|---|
| 321 | 515 MPa | 205 MPa | 40% | 217 HBW |
Available finishes
| Pickled | Heat-tint and oxide removed after welding or heat treatment. The standard supply condition for industrial pipe. |
|---|---|
| Bright annealed | Reflective surface for visible or hygienic service. |
| Polished | Mechanical polish to a specified grit for architectural or sanitary use. |
Applications
- Exhaust and manifold systems
- Heat exchangers
- Refinery and petrochemical piping
- Furnace parts
- Aircraft components
Quality documents
Every shipment includes an EN 10204 3.1 mill test certificate stating the heat number, chemical composition and mechanical properties. PMI and third-party pre-shipment inspection are available on request.
How quality is controlled321 questions
Why use 321 instead of 304 for high-temperature work?
Titanium in 321 combines with carbon, preventing chromium carbide precipitation in the 425–815 °C range. That keeps chromium in solution for corrosion resistance and lets the grade stay in continuous service at higher temperatures than 304.
Is 321 suitable for welding?
Yes, and that is one of its main advantages: the titanium stabilisation protects the heat-affected zone from intergranular corrosion, so post-weld solution annealing is normally unnecessary for moderate service conditions.
What is the difference between 321 and 347?
Both are stabilised grades. 321 uses titanium, 347 uses niobium plus tantalum. They are often interchangeable in high-temperature service, and the choice usually follows the project specification or the availability of the required product form.
Packing and loading
- Export packing to the method stated on the quotation
- Marking with grade, size, heat number and order reference
- Moisture protection for sea freight
- Loading photographs supplied before departure
Related products
304 / 304L
304 (UNS S30400, EN 1.4301) is the most widely used austenitic stainless steel: 18% chromium, 8% nickel, non-magnetic in the annealed condition and suitable for food-contact, architectural and general fabrication.
View specifications
316L
316L (UNS S31603, EN 1.4404) adds 2–3% molybdenum to the 18/8 base, raising resistance to pitting and crevice corrosion in chlorides.
View specifications
C12200
Refrigeration and air-conditioning copper tube made to DIN 8905 and EN 12735 T1/T2 from 99.9% copper, blank inside, clean and dry — supplied in pancake coils and straight lengths in soft, half-hard and hard temper..
View specificationsNeed this grade in another form?
321 is also supplied in the other forms listed for stainless steel.